Adhesive mixture for facing surfaces with tiles up to 600x600 mm in size — TM 10
External and internal
Field of application:
For laying all types of ceramic and clinker tiles, as well as natural stone indoors and outdoors, on walls and floors, in dry and wet areas. For facing with large-format tiles 1200*600 mm, with moisture absorption less than 0.5%. Especially suitable for heated floors and thin translucent plates, glass mosaic, light marble, etc., for facing stairs and stairwells, as well as surfaces, subject to intense mechanical deformations. Effective on foundations, subject to periodic deformation due to moisture and extension(indoor pools and tanks, showers, balconies, terraces, heated floors, etc.), on terraces and balconies.
Features:
Advantages:
from 20 min
Storage |
Cement, mineral fillers, |
Water consumption for 25 kg |
7.0....7.5 |
Consumption of dry mixture per 1 m² |
Approximately 1.7 kg |
Expiry date, min | At least 60 |
Open time, min | At least 20 |
Adjustment time, min | At least 10 |
Adhesion strength to the base after: |
Not less than 1.0 |
Coarseness of aggregate, mm | Not more than 0.63 |
Displacement of the material to be fixed |
Not more than 0.5 |
Compressive strength (after 28 days), Mpa | Not less than 10.0 |
Application temperature | From +5 ⁰С to +30 ⁰С |
Operating temperature | From -30 ⁰С to +40 ⁰С |
The time of possible technological |
Not before 48 |
The foundation is prepared in accordance with DSTU-NB A.3.1- 23:2013 and DSTU-NB V.2.6-212:2016. The surface of the base must be dry, strong, even, with low and uniform water absorption. Before applying the dry mixture, the surface is cleaned of dust, oil stains and other substances that reduce adhesion. Surfaces made of porous concrete, as well as gypsum and smooth concrete surfaces should be treated with a primer. Leave primed surfaces for at least 4 hours before starting cladding.
Preparation of mortar mixture: pour water into a clean container (water temperature from +15 °C to +25 °C) at the rate of 0.28-0.30 l (l) per 1 kg (kg) of dry mixture (7.0-7 .5 l (l) per 25 kg (kg)), gradually add the dry mixture and mix with a low-speed mixer until a homogeneous mass without lumps is obtained. After 5 minutes mix again.
The use of dry mixture is recommended at temperatures from +5 °C to +30 °C and relative air humidity not higher than 65%. Eyes and skin should be protected during work. If the mixture gets into the eyes, it is necessary to immediately wash them with water and consult a doctor.
On bases with deformation seams, the latter must be additionally duplicated in the facing, followed by their filling with elastic sealants. When performing external work, a combined method is used for fixing tiles: the mortar mixture is applied to the surface in a layer, the thickness of which should correspond to the size of the grater tooth, and to the tile in a layer of up to 1 mm, evenly over the entire surface.
The mortar mixture is applied in a thin layer to the prepared base using a metal spatula or grater and smoothed with a toothed spatula. At one time, such amount of solution is applied that can be used within 15 minutes. The tile was not previously repl
Paper bags with an inner polyethylene layer of 25 kg.
The mixture must be stored in a branded sealed package in a dry room, on pallets. The shelf life is 12 months from the date of manufacture indicated on the package.
On average, 1.7 kg of glue is used per 1 m2, depending on the thickness of the applied layer and the condition of the surface.